| 性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | |
| 比重 | ASTMD792 | 1.12 | g/cm3 | |
| 熔流率(熔体流动速率) | 190°C/21.6kg | ASTMD1238 | 40to60 | g/10min |
| 熔流率(熔体流动速率) | 190°C/8.7kg | ASTMD1238 | 10to20 | g/10min |
| 拉伸模量(注塑) | ASTMD412 | 20.7 | MPa | |
| 弯曲模量(注塑) | ASTMD790 | 29.0 | MPa | |
| 泰伯耐磨性 | ASTMD1044 | 30.0 | mg | |
| Abrasion-DIN | DIN53516 | 25 | mm3 | |
| 弹性体 | TestMethod | NominalValue | Unit | |
| 拉伸应力(100%应变) | ASTMD412 | 9.65 | MPa | |
| 拉伸应力(300%应变) | ASTMD412 | 21.4 | MPa | |
| 抗张强度 | ASTMD412 | 35.9 | MPa | |
| 伸长率(断裂) | ASTMD412 | 530 | % | |
| 撕裂强度2 | ASTMD624 | 110 | kN/m | |
| 压缩永久变形 | 23°C,22hr | ASTMD395B | 25 | % |
| 压缩永久变形 | 70°C,22hr | ASTMD395B | 45 | % |
| 肖氏硬度(邵氏A) | ASTMD2240 | 85 | ||
| 玻璃转化温度 | InternalMethod | -38.0 | °C | |
| 维卡软化温度 | ASTMD1525 | 100 | °C | |
| SofteningPoint-DMA | InternalMethod | 66 | °C | |
| UL阻燃等级(1.5mm) | UL94 | HB | ||
TPU聚醚 1185A10X塑料供应商,长期销售德国巴斯夫生产的TPU聚醚原料,以上是“TPU聚醚 Elastollan® 1185A10X”塑胶料的物性表参数.近期代理商可转仓交易:荷兰Witcom PP Witcom PP C/2G-EC-EM 填料,玻璃纤维增强材料,10%填料按重量.
澳大利亚PolyPacific PP Retpol® 7555 HS UV2
日本美拉龙 TPU合金 Mirakutoran® TPU E880
意大利API TPU聚脂 apilon 52c® C S60 LV
美国Teknor Apex TPE Medalist™ MD-12243
美国Elastocon TPE Elastocon® 2840B
中国江苏鼎启钟华 TPE Jiangsu Sinarise ZM808 阻燃性 电线电缆应用
日本三菱 TPV Trexprene® A35BU
意大利兰蒂奇 SEBS Heraflex® A 35-13-40 低密度 汽车领域的应用
美国塞拉尼斯 PPS Fortron® 0205 良好的流动性,中等粘性,热稳定性良好,耐化学性良好 复合
德国赢创(德固赛) PEEK VESTAKEEP® Care M40R
日本住友 EPDM ESPRENE EPDM 6101
● TPU聚醚 德国巴斯夫 Elastollan 1190A50
● TPU聚醚 美国路博润 Estane 58212 TPU
● TPU聚醚 德国巴斯夫 Elastollan 1185 A 15 000
抗微生物,低温下的柔性,耐水解性,注射成型
● TPU聚醚 德国科思创 Desmopan DP 9395AU
抗微生物,耐水解性,低温下的柔性,挤出,注射成型
● TPU聚醚 德国巴斯夫 Elastollan 1185 A