| 性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | |
| 比重 | ASTMD792 | 1.20 | g/cm3 | |
| 熔流率(熔体流动速率) | 190°C/3.8kg | ASTMD1238 | 15to25 | g/10min |
| 熔流率(熔体流动速率) | 190°C/8.7kg | ASTMD1238 | 40to60 | g/10min |
| 拉伸模量(注塑) | ASTMD412 | 24.8 | MPa | |
| 弯曲模量(注塑) | ASTMD790 | 22.1 | MPa | |
| 泰伯耐磨性 | ASTMD1044 | 40.0 | mg | |
| Abrasion-DIN | DIN53516 | 10 | mm3 | |
| 弹性体 | TestMethod | NominalValue | Unit | |
| 拉伸应力(100%应变) | ASTMD412 | 5.31 | MPa | |
| 拉伸应力(300%应变) | ASTMD412 | 12.7 | MPa | |
| 抗张强度 | ASTMD412 | 33.1 | MPa | |
| 伸长率(断裂) | ASTMD412 | 610 | % | |
| 撕裂强度2 | ASTMD624 | 85.8 | kN/m | |
| 压缩永久变形 | 23°C,22hr | ASTMD395B | 20 | % |
| 压缩永久变形 | 70°C,22hr | ASTMD395B | 50 | % |
| 肖氏硬度(邵氏A) | ASTMD2240 | 78 | ||
| 玻璃转化温度 | InternalMethod | -27.0 | °C | |
| 维卡软化温度 | ASTMD1525 | 64.0 | °C | |
| SofteningPoint-DMA | InternalMethod | 66 | °C | |
TPU聚脂 880A-13N塑料供应商,长期销售德国巴斯夫生产的TPU聚脂原料,以上是“TPU聚脂 Elastollan® 880A-13N”塑胶料的物性表参数.近期代理商可转仓交易:美国Washington Penn PP WPP PP PRC25MF1.2C 填料,Washington,Penn,美国Washington,Penn.汽车领域的应用
美国朗讯 PP Primefin V525H 冲击改性
美国Greene 氟橡胶 Greene FKM 938
比利时索尔维 氟橡胶 Tecnoflon® P 459
德国科思创 TPU聚醚 Texin® 970 U 可粘结性,嵌段共聚物,耐化学性良好,柔软,注射成型
美国Star TPE StarPrene® 6101-70
英国ELASTO TPE Dryflex® 9012
美国盛禧奥 TPO Polypropylene DLGF9411.00 填料,长玻璃纤维,40%填料按重量.
美国Network Polymers TPE Softflex® 8795 包覆成型
意大利SO.F.TER SEBS Laprene® 8ST193A80/T2 注射成型
中国深圳盛嘉伦 TPE Gallonprene® GP540-8005 高弹性,优良外观,无卤,型材挤出成型,挤出 电线电缆应用,型材,管件
英国ELASTO SBS Mediprene® 880161
美国RTP PEI RTP 2105 L 填料,玻璃纤维增强材料,30%填料按重量.
美国RTP PEEK RTP 2283 LF 填料,碳纤维增强材料,20%填料按重量.
● TPU聚脂 德国巴斯夫 Elastollan R 3000
● TPU聚脂 美国RTP RTP ESD A 1200 90A
抗静电性,注射成型
● TPU聚脂 德国巴斯夫 Elastollan S60DN
● TPU聚脂 美国RTP RTP 1207-70A
填料:玻璃纤维增强材料, 40% 填料按重量。
● TPU聚脂 美国路博润 PEARLCOAT 127K