抗氧化性,可加工性,良好 吹塑薄膜,流延薄膜,薄膜挤出 | |
薄膜,拉伸缠绕 | |
性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | |
密度 | ASTMD1505 | 0.911 | g/cm3 | |
熔流率(熔体流动速率)(190°C/2.16kg) | ASTMD1238 | 2.0 | g/10min | |
抗张强度(断裂) | ASTMD638 | 18.6 | MPa | |
伸长率(断裂) | ASTMD638 | 960 | % | |
薄膜厚度-经测试 | 20 | um | ||
抗张强度 | MD:断裂,20um | ASTMD882 | 39.2 | MPa |
抗张强度 | TD:断裂,20um | ASTMD882 | 34.3 | MPa |
伸长率 | MD:断裂,20um | ASTMD882 | 600 | % |
伸长率 | TD:断裂,20um | ASTMD882 | 800 | % |
落锤冲击(20um) | ASTMD1709 | 120 | g | |
TensileTearStrength | MD:20.0um | ASTMD1004 | 117.7 | kN/m |
TensileTearStrength | TD:20.0um | ASTMD1004 | 122.6 | kN/m |
薄膜厚度-经测试 | 20 | um | ||
抗张强度 | MD:断裂,20um | ASTMD882 | 39.2 | MPa |
抗张强度 | TD:断裂,20um | ASTMD882 | 34.3 | MPa |
伸长率 | MD:断裂,20um | ASTMD882 | 600 | % |
伸长率 | TD:断裂,20um | ASTMD882 | 800 | % |
落锤冲击(20um) | ASTMD1709 | 120 | g | |
TensileTearStrength | MD:20.0um | ASTMD1004 | 117.7 | kN/m |
TensileTearStrength | TD:20.0um | ASTMD1004 | 122.6 | kN/m |
脆化温度 | ASTMD746 | <-76.0 | °C | |
维卡软化温度 | ASTMD1525 | 96.0 | °C | |
熔融峰值温度 | 内部方法 | 121 | °C | |
雾度(20.0um) | ASTMD1003 | 2.0 | % |
LLDPE HANWHA LLDPE 3325W塑料供应商,长期销售韩国Hanwha(韩华)生产的LLDPE原料,以上是“LLDPE HANWHA LLDPE 3325W”塑胶料的物性表参数.近期代理商可转仓交易:美国朗讯 PP均聚 Lucent PP TPP-0310-20 填料,滑石填料,20%填料按重量.
美国利安德巴塞尔 PP均聚 Hostacom HKP 2034D NAT
美国舒尔曼ICO Polymers PP共聚 ICORENE® N4505 无规共聚物 密封件
美国埃克森美孚化工 PP均聚 ExxonMobil™ PP8255E1 可加工性良好,抗撞击性良好,中等分子量,成核的,均衡的,刚性/韧性,良好的耐热老化性能,吹塑成型,复合,注射成型 复合,汽车领域的应用,电器用具
美国利安德巴塞尔 PP共聚 Moplen RP210G
美国利安德巴塞尔 PP共聚 Hifax CA 1110 G4 LS 1740
日本普瑞曼 LLDPE Evolue™ SP2520 光学性能,快的成型周期,刚性良好,吹塑薄膜 农业应用,工业应用,薄膜,层压板
美国利安德巴塞尔 LDPE Petrothene® NA338202 食品接触的合规性,低摩擦系数,刚性良好,清晰度高,流延薄膜 流延薄膜,薄膜
美国塞拉尼斯 LDPE AT 418 内缩量低,良好粘结性,挤出涂层,层压法 层压板,涂层应用
美国杜邦 HDPE Fusabond® E265 高密度
美国Entec HDPE Hypel® PEHD20/.953 高密度
美国RTP PP 103 FR A 阻燃,注塑
● LLDPE 美国陶氏 DOWLEX 2517
● LLDPE 韩国韩华 CHBA-8280TG
挤出
● LLDPE 美国陶氏 SC 2107G
挤出
● LLDPE 日本宇部 UMERIT 2000F
● LLDPE 韩国DAELIM(大林) Daelim Po1y LL-34
可加工性良好,清晰度高,高抗结块性