高强度,可加工性,良好,抗氧化性,光滑性,光学性能 流延薄膜,薄膜挤出 | |
拉伸缠绕,薄膜 | |
性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | |
密度 | ASTMD1505 | 0.923 | g/cm3 | |
熔流率(熔体流动速率)(190°C/2.16kg) | ASTMD1238 | 3.2 | g/10min | |
抗张强度(断裂) | ASTMD638 | 34.3 | MPa | |
伸长率(断裂) | ASTMD638 | 900 | % | |
薄膜厚度-经测试 | 20 | um | ||
抗张强度 | MD:断裂,20um | ASTMD882 | 44.1 | MPa |
抗张强度 | TD:断裂,20um | ASTMD882 | 39.2 | MPa |
伸长率 | MD:断裂,20um | ASTMD882 | 750 | % |
伸长率 | TD:断裂,20um | ASTMD882 | 850 | % |
落锤冲击(20um) | ASTMD1709B | 200 | g | |
TensileTearStrength | MD:20.0um | ASTMD1004 | 117.7 | kN/m |
TensileTearStrength | TD:20.0um | ASTMD1004 | 127.5 | kN/m |
薄膜厚度-经测试 | 20 | um | ||
抗张强度 | MD:断裂,20um | ASTMD882 | 44.1 | MPa |
抗张强度 | TD:断裂,20um | ASTMD882 | 39.2 | MPa |
伸长率 | MD:断裂,20um | ASTMD882 | 750 | % |
伸长率 | TD:断裂,20um | ASTMD882 | 850 | % |
落锤冲击(20um) | ASTMD1709B | 200 | g | |
TensileTearStrength | MD:20.0um | ASTMD1004 | 117.7 | kN/m |
TensileTearStrength | TD:20.0um | ASTMD1004 | 127.5 | kN/m |
脆化温度 | ASTMD746 | <-76.0 | °C | |
维卡软化温度 | ASTMD1525 | 105 | °C | |
熔融峰值温度 | 内部方法 | 125 | °C | |
雾度(20.0um) | ASTMD1003 | 2.0 | % |
LLDPE HANWHA LLDPE HS1700塑料供应商,长期销售韩国Hanwha(韩华)生产的LLDPE原料,以上是“LLDPE HANWHA LLDPE HS1700”塑胶料的物性表参数.近期代理商可转仓交易:意大利TECNOPOL PP均聚 OMIKRON BG 73 NAT
沙伯基础 PP均聚 SABIC® PP 48M10
沙伯基础 PP均聚 SABIC® PP 49MK45
中国上海赛科石油 PP共聚 SECCO K8703 共聚物
沙特阿拉伯Rabigh LLDPE Petro Rabigh PE FS150A 抗撞击性良好,韧性良好,清晰度高,薄膜挤出 拉伸缠绕,层压板,薄膜
美国利安德巴塞尔 PP共聚 Hostacom TRC 352N G22375
以色列普利朗 PP共聚 RAMOFIN PPC101 热稳定性,注射成型
日本三井 LDPE MIRASON™ MV660 良好的柔韧性,高ESCR,抗应力开裂,挤出 片材
中国北京燕山石化 LDPE Yanshan PE LD362 薄膜挤出 农业应用,多层薄膜,层压板,包装,薄膜,袋子
俄罗斯Nizhnekamskneftekhim HDPE NEFTEKHIM PE 6254N
匈牙利MOL HDPE TIPELIN® 7111S
美国RTP HDPE RTP 702 Z 填料,玻璃纤维增强材料,15%填料按重量.
上海华合 PA66 PA66+15GF+25GB 15%玻纤增强,25%玻璃微珠
美国塞拉尼斯 PPS CF30-01 刚性高,抗撞击性良好
● LLDPE 沙特sabic PCG6118NE
低密度光学性能己烯共聚单体 抗氧化性抗撞击性,高良好的撕裂强度
● LLDPE 科威特EQUATE EHS-7066
薄膜
● LLDPE 美国杜邦 4105
良好粘结性
● LLDPE 日本三菱 UF420A
薄膜
● LLDPE 埃克森美孚 LL 8555.67
提供良好的加工性能,尺寸控制,白度和低翘曲。这种树脂是非常适合用于需要良好的表面外观和环境应力龟裂,刚度最佳平衡,韧性。