性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | |
比重 | ASTMD792 | 1.59 | g/cm3 | |
收缩率-流动 | ASTMD955 | 0.45to0.85 | % | |
抗张强度2(屈服) | ASTMD638 | 128 | MPa | |
伸长率(断裂) | ASTMD638 | 3.0 | % | |
弯曲模量3 | ASTMD790 | 7900 | MPa | |
弯曲强度3(屈服) | ASTMD790 | 197 | MPa | |
泰伯耐磨性(1000Cycles,1000g,CS-17转轮) | ASTMD1044 | 40.0 | mg | |
悬壁梁缺口冲击强度 | ASTMD256 | 90 | J/m | |
悬壁梁缺口冲击强度 | ASTMD256 | 640 | J/m | |
ReverseNotchIzodImpact | ASTMD256 | 700 | J/m | |
洛氏硬度(M级) | ASTMD785 | 85 | ||
DeflectionTemperatureUnderLoad(0.45MPa,Annealed,6.35mm) | ASTMD648 | 165 | °C | |
载荷下热变形温度(1.8MPa,退火,6.35mm) | ASTMD648 | 160 | °C | |
线形热膨胀系数-流动(20到80°C) | ASTMD696 | 4.0E-5 | cm/cm/°C | |
RTIElec(0.75mm) | UL746 | 50.0 | °C | |
RTIImp(0.75mm) | UL746 | 50.0 | °C | |
RTIStr(0.75mm) | UL746 | 50.0 | °C | |
表面电阻率 | ASTMD257 | 1.0E+14 | ohms | |
体积电阻率 | ASTMD257 | 1.0E+16 | ohmscm | |
介电强度 | ASTMD149 | 23 | kV/mm | |
耐电弧性 | ASTMD495 | 125 | sec | |
UL阻燃等级(0.75mm,All) | UL94 | HB |
POM共聚 GC225塑料供应商,长期销售韩国LG化学生产的POM共聚原料,以上是“POM共聚 Lucel® GC225”塑胶料的物性表参数.近期代理商可转仓交易:中国广东银禧 TPE SILVER® SA-5206
美国威凯 TPE Sevrene® 3085-70A
中国深圳盛嘉伦 TPE Gallonprene® GP320-55 无卤,高弹性 柔软的把手,电器用具,包覆成型,工业应用
巴西Petropol PP+EPDM Unipren® Elastomers B3 NTLA010 55A UP310 高耐热性,耐气候影响性能良好
墨西哥化工 SEBS Evoprene™ G 3292
土耳其Elastron SEBS Elastron® G G300.A55.B 嵌段共聚物,柔软,耐化学性良好,可粘结性,注射成型
美国杜邦 EVA Elvax® 3170SHB
德国赢创(德固赛) PPA VESTAMID® HTplus M1933
美国塞拉尼斯 EVA Ateva® 9030 共聚物 太阳能电池板
德国莱曼 PEEK LUVOCOM® 1105-8161 填料,碳纤维增强材料.轴承,泵件,衬套,汽车领域的应用,纺织应用,航空航天应用,齿轮,医疗/护理用品,工程配件
美国塞拉尼斯 LCP CoolPoly® D5502
沙伯基础 PPO(PPE) NORYL™ RN0712 resin
美国Techmer POM共聚 Plaslube® POM CO CF10 TL10 BK 填料,碳纤维增强材料,10%填料按重量.
德国科思创 PC Bayblend® T45 PG 可电镀
沙伯基础 PC AVP™ FLLS0CP 阻燃性,注射成型
● POM共聚 美国RTP RTP 801 GB 20 CC
填料:玻璃珠, 20% 填料按重量,玻璃纤维增强材料, 10% 填料按重量。
● POM共聚 韩国工程塑料 Kepital F30-02
共聚物,良好的成型性能,低粘度,耐磨损性良好,良好的抗蠕变性,良好的流动性,耐疲劳性能,热稳定性良好,耐化学性良好,注射成型
● POM共聚 日本宝理 DURACON WR-01
防潮性,注射成型
● POM共聚 日本宝理 DURACON EB-08
导电,抗静电性,注射成型
● POM共聚 沙伯基础 LNP LUBRICOMP KFI12 compound
填料:玻璃纤维增强材料, 10% 填料按重量。