性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | |
比重 | ASTMD792 | 1.34 | g/cm3 | |
熔流率(熔体流动速率)(300°C/1.2kg) | ASTMD1238 | 8.0 | g/10min | |
收缩率-流动 | ASTMD955 | 0.30to0.50 | % | |
吸水率(23°C,24hr) | ASTMD570 | 0.12 | % | |
抗张强度(屈服) | ASTMD638 | 98.1 | MPa | |
伸长率(断裂) | ASTMD638 | 3.0 | % | |
弯曲模量 | ASTMD790 | 4900 | MPa | |
弯曲强度(屈服) | ASTMD790 | 137 | MPa | |
悬壁梁缺口冲击强度(23°C,3.18mm) | ASTMD256 | 98 | J/m | |
洛氏硬度(R级) | ASTMD785 | 122 | ||
载荷下热变形温度(0.45MPa,未退火) | ASTMD648 | 151 | °C | |
载荷下热变形温度(1.8MPa,未退火) | ASTMD648 | 150 | °C | |
线形热膨胀系数-流动 | ASTMD696 | 2.3E-5 | cm/cm/°C | |
体积电阻率 | ASTMD257 | 4.0E+16 | ohmscm | |
介电强度 | ASTMD149 | 31 | kV/mm | |
介电常数 | ASTMD150 | 3.05 | ||
耗散因数 | ASTMD150 | 9.7E-3 | ||
耐电弧性 | ASTMD495 | 120 | sec | |
UL阻燃等级 | UL94 | HB |
PC Compound 3025G20塑料供应商,长期销售韩国三养生产的PC原料,以上是“PC TRIREX® Compound 3025G20”塑胶料的物性表参数.近期代理商可转仓交易:意大利Taro Plast SEBS NILFLEX® SH A90 MC009
意大利Guarniflon PTFE Flontech® FT-910-ST
土耳其Elastron SBS Elastron® D D400.A50.T 可粘结性,嵌段共聚物,柔软,注射成型
Generic PP弹性体 Generic PP Elastomer
日本三井 EPDM Mitsui EPT™ 3092M
中国浙江新和成 PPS NHU-PPS 21330C/F
日本JSR EPDM JSR EPR EP922P 抗结块性 塑料改性
美国普立万 POM共聚 Edgetek™ AT-000/000 GREY VN-3581
以色列普利朗 POM均聚 RAMTAL PMH2022 通用,注射成型 通用
韩国LG化学 PC Lupoy® GP5206F
美国Ovation PC RIGITRON 10001 高拉伸强度,冲击改性,高刚性
美国普立万 PC LubriOne™ PC-30GF/15T-2S BLACK 填料,玻璃纤维增强材料,30%填料按重量.
日本三菱 PC NOVAREX® M7020AD2 光学数据存储
日本电气化学 PC DENKA Polymer Alloy HS-K190 抗撞击性高
美国杜邦 PBT Crastin® SO653 NC010 填料,玻璃珠,20%填料按重量.
● PC 三菱工程塑料 7025G30
30%GF
● PC 韩国三养 3022U(E)
透明,阻燃,电子电器部件,汽车部件,注塑
● PC 美国RTP RTP 380.5
填料:碳纤维增强材料, 5.0% 填料按重量。
● PC 三菱工程塑料 7030U-8
注塑
● PC 日本出光 IN2200S
特性:提高了耐水解性