| 热稳定性 注射成型 | 自然色,黑色 |
| 填料:滑石填料, 20% 填料按重量。 | |
| 性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | |
| 比重 | ASTMD792 | 1.05 | g/cm3 | |
| 收缩率-流动(3.18mm) | ASTMD955 | 1.2 | % | |
| 吸水率(23°C,24hr) | ASTMD570 | 0.030 | % | |
| 洛氏硬度(R级) | ASTMD785 | 90 | ||
| 拉伸模量 | ASTMD638 | 2550 | MPa | |
| 抗张强度 | ASTMD638 | 34.5 | MPa | |
| 伸长率(断裂) | ASTMD638 | 5.0 | % | |
| 弯曲模量 | ASTMD790 | 2140 | MPa | |
| 弯曲强度 | ASTMD790 | 53.8 | MPa | |
| 压缩强度 | ASTMD695 | 47.6 | MPa | |
| 悬壁梁缺口冲击强度(3.18mm) | ASTMD256 | 32 | J/m | |
| 无缺口悬臂梁冲击(3.18mm) | ASTMD4812 | 250 | J/m | |
| 载荷下热变形温度 | 0.45MPa,未退火 | ASTMD648 | 121 | °C |
| 载荷下热变形温度 | 1.8MPa,未退火 | ASTMD648 | 71.1 | °C |
| 线形热膨胀系数-流动 | ASTMD696 | 5.9E-5 | cm/cm/°C | |
| 导热系数 | ASTMC177 | 0.26 | W/m/K | |
| 体积电阻率 | ASTMD257 | 1.0E+16 | ohmscm | |
| 介电强度 | ASTMD149 | 20 | kV/mm | |
| 介电常数(1MHz) | ASTMD150 | 2.40 | ||
| 耗散因数(1MHz) | ASTMD150 | 4.0E-3 | ||
| 耐电弧性 | ASTMD495 | 125 | sec | |
| UL阻燃等级(1.6mm,ValuesperRTPCompanytesting.) | UL94 | HB | ||
PP均聚 RTP 128 Z塑料供应商,长期销售美国RTP生产的PP均聚原料,以上是“PP均聚 RTP 128 Z”塑胶料的物性表参数.近期代理商可转仓交易:伊朗Pooya PP均聚 POYAD SS102
巴西布拉斯科 PP均聚 Braskem PP C758-80NA 抗静电性,食品接触的合规性,抗冲共聚物,成核的,注射成型 薄壁部件
奥地利北欧化工 PP均聚 Borclean™ HC318BF 表面光洁度不光滑,刚性良好,可加工性良好,无添加剂,均聚物,纯度高,可回收材料,热稳定性良好,薄膜挤出 双向拉伸薄膜,电气元件,薄膜
意大利AD COMPOUND PP均聚 PERLER® N09X4001B01 填料,矿物填料,40%填料按重量.
美国特诺尔爱佩斯 PP共聚 SINPOLENE TPP2030 填料,Teknor,美国特诺尔爱佩斯.
美国The Matrixx Group PP共聚 Matrixx TPP2B40 填料,The,Matrixx,Group,美国The,Matrixx,Group.
美国利安德巴塞尔 PP共聚 Hifax EKC 200P C11306
美国华美化学 LLDPE HIFOR Xtreme® SC74875
美国舒尔曼 LDPE ASI POLYETHYLENE CP 769-01 NATURAL 良好的热封性,可加工性良好,挤出,吹塑成型
俄罗斯喀山石化 LDPE Kazan LDPE 153 VSKM 铜接触稳定,挤出 电线电缆应用,电缆护套
日本三井 HDPE LUBMER™ L4000 轴承,汽车内部零件,齿轮
美国RTP LDPE RTP 799 A X 143512 EG 静电放电保护,抗静电性,挤出,注射成型
● PP均聚 台湾台化 Formolene 6630A
● PP均聚 美国舒尔曼 POLYFORT FPP 30 GFC
填料:玻璃纤维增强材料, 30% 填料按重量。
● PP均聚 台湾台化 YUNGSOX PP 1120D
均聚物,刚性良好,高耐热性
● PP均聚 韩国DAELIM(大林) Daelim Po1y PP-184
气味低到无,窄分子量分布,均聚物
● PP均聚 美国舒尔曼 PERCOM MC12
通用,抗冲共聚物