| 润滑,热稳定性 注射成型 | 黑色,自然色 |
| 性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | |
| 比重 | ASTMD792 | 1.27 | g/cm3 | |
| 收缩率-流动(3.18mm) | ASTMD955 | 1.4 | % | |
| 吸水率(23°C,24hr) | ASTMD570 | 0.80 | % | |
| 洛氏硬度(R级) | ASTMD785 | 118 | ||
| 拉伸模量 | ASTMD638 | 2830 | MPa | |
| 抗张强度 | ASTMD638 | 62.1 | MPa | |
| 伸长率(断裂) | ASTMD638 | 3.0 | % | |
| 弯曲模量 | ASTMD790 | 2340 | MPa | |
| 弯曲强度 | ASTMD790 | 97.9 | MPa | |
| 压缩强度 | ASTMD695 | 32.4 | MPa | |
| 摩擦系数(与金属-动态) | ASTMD1894 | 0.060 | ||
| 悬壁梁缺口冲击强度(6.35mm) | ASTMD256 | 43 | J/m | |
| 无缺口悬臂梁冲击(6.35mm) | ASTMD4812 | 430 | J/m | |
| 载荷下热变形温度 | 0.45MPa,未退火 | ASTMD648 | 210 | °C |
| 载荷下热变形温度 | 1.8MPa,未退火 | ASTMD648 | 104 | °C |
| 线形热膨胀系数-流动 | ASTMD696 | 8.1E-5 | cm/cm/°C | |
| 导热系数 | ASTMC177 | 0.26 | W/m/K | |
| 体积电阻率 | ASTMD257 | 1.0E+15 | ohmscm | |
| 介电强度 | ASTMD149 | 20 | kV/mm | |
| 介电常数(1MHz) | ASTMD150 | 3.70 | ||
| 耗散因数(1MHz) | ASTMD150 | 0.015 | ||
| UL阻燃等级(1.6mm) | UL94 | HB | ||
PA66 RTP 200 TFE 18 SI 2 HS塑料供应商,长期销售美国RTP生产的PA66原料,以上是“PA66 RTP 200 TFE 18 SI 2 HS”塑胶料的物性表参数.近期代理商可转仓交易:韩国工程塑料 POM共聚 Kepital® TS-25A 润滑,耐磨损性良好
瑞士英力士 PC+ABS Novodur® Ultra 4115
比利时Ravago PC Hybrid S464G10 填料,玻璃纤维增强材料,10%填料按重量.
德国科思创 PC Makrolon® 6717 脱模性能良好,阻燃性,粘度高,挤出,注射成型
比利时Ravago PC Hybrid S466 韧性良好,耐低温冲击
韩国乐天化学 PC Infino LM-1090 阻燃性
美国RTP PC RTP 399 X 138754 C 静电放电保护,静态导电,UV/Stabilized,注射成型
德国Kunststoff PBT GERMADUR SZ-5223 抗撞击性高
中国上海锦湖日丽 PBT KumhoSunny PBT 3730FG-NH
美国Custom Resins PA66 6/Nylene® 4223 HS UV 共聚物 汽车领域的应用
韩国三养 PBT TRIBIT® 1500G40
美国普立万 PA66 Stat-Tech™ NN-20CF/000 Black HS
意大利兰蒂奇 PA66 Radilon® A CV500 100 NAT 填料,玻璃珠,50%填料按重量.
英国4PLAS PA66 4MID® 9A22120 填料,玻璃纤维增强材料,20%填料按重量.
比利时索尔维 PA66 TECHNYL® A 21T3 V25 BLACK 15N
● PA66 日本旭化成 Leona 90G33
填料:玻璃纤维增强材料, 33% 填料按重量。
● PA66 韩国LG化学 Lumid GP2151BF
填料:玻璃纤维增强材料, 15% 填料按重量。
● PA66 韩国LG化学 Lumid GP2430B(W)
填料:玻璃纤维增强材料, 43% 填料按重量。
● PA66 韩国工程塑料 Kepamid 2320CF