| 高强度 注射成型 | |
| 填料:玻璃纤维增强材料, 13% 填料按重量。 | |
| 性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | |
| 比重 | ASTMD792 | 1.22 | g/cm3 | |
| 收缩率-流动 | ASTMD955 | 0.70 | % | |
| 吸水率(23°C,24hr) | ASTMD570 | 0.90 | % | |
| 洛氏硬度(R级) | ASTMD785 | 120 | ||
| 拉伸模量 | ASTMD638 | 5170 | MPa | |
| 抗张强度 | 屈服 | ASTMD638 | 103 | MPa |
| 抗张强度 | —— | ASTMD638 | 110 | MPa |
| 伸长率(断裂) | ASTMD638 | 3.5 | % | |
| 弯曲模量 | ASTMD790 | 4830 | MPa | |
| 弯曲强度 | —— | ASTMD790 | 172 | MPa |
| 弯曲强度 | 屈服 | ASTMD790 | 152 | MPa |
| 压缩强度 | ASTMD695 | 103 | MPa | |
| 悬壁梁缺口冲击强度(3.18mm) | ASTMD256 | 48 | J/m | |
| 无缺口悬臂梁冲击(3.18mm) | ASTMD4812 | 430 | J/m | |
| 载荷下热变形温度 | 0.45MPa,未退火 | ASTMD648 | 249 | °C |
| 载荷下热变形温度 | 1.8MPa,未退火 | ASTMD648 | 243 | °C |
| 线形热膨胀系数-流动 | ASTMD696 | 4.7E-5 | cm/cm/°C | |
| 导热系数 | ASTMC177 | 0.42 | W/m/K | |
| 体积电阻率 | ASTMD257 | 1.0E+14 | ohmscm | |
| 介电强度 | ASTMD149 | 20 | kV/mm | |
| 介电常数(1MHz) | ASTMD150 | 3.70 | ||
| 耗散因数(1MHz) | ASTMD150 | 0.020 | ||
| 耐电弧性(1.59mm) | ASTMD495 | 100 | sec | |
| UL阻燃等级(1.6mm) | UL94 | HB | ||
PA66 RTP 201.3塑料供应商,长期销售美国RTP生产的PA66原料,以上是“PA66 RTP 201.3”塑胶料的物性表参数.近期代理商可转仓交易:美国RTP PC RTP 4300 S-1000 Z 注射成型
德国BARLOG plastics POM共聚 KEBAFORM® C 909 WR
沙伯基础 PPO(PPE) NORYL™ WCD891B resin
美国普立万 PC Stat-Tech™ PC-10CF/000 FR V0 BLK035 填料,碳纤维增强材料,10%填料按重量.
日本三菱 PC Iupilon® EGN2020KR 填料,玻璃纤维增强材料,20%填料按重量.
德国科思创 PC Makrolon® LED2045 低粘度,脱模性能良好,清晰度高,注射成型 照明应用
中国广东银禧 PC SILVER® PC2540.DF
美国Polymer Resources PC PRL PC-FR1-D 阻燃性,耐热性中等,粘度高,流动性低,自熄,抗撞击性高,注射成型
美国KMI PC KMI PC/ABS 2500
以色列普利朗 PBT RAMSTER PF713 抗紫外线性能良好,中等粘性,注射成型
土耳其Eurotec PBT Tecodur® PB70 NL 注射成型
比利时Ravago PA66 Hylon® N1200TL 冲击改性
国别不详 PA66 Taizhou Plastic PA66
美国奥升德(首诺) PA66 Vydyne® R535J BK0678
韩国万都新材 PA66 TEKAMID™ TA210L 脱模性能良好
● PA66 韩国工程塑料 Kepamid 2333GB
填料:玻璃珠, 30% 填料按重量。
● PA66 美国奥升德(首诺) Vydyne R525H Nat
● PA66 美国RTP ESD A 200H
注塑
● PA66 韩国可隆 KN333NW
尺寸稳定性良好、抗撞击性良好