| 注射成型 | |
| 性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | |
| 比重 | ASTMD792 | 1.14 | g/cm3 | |
| 熔流率(熔体流动速率)(224°C/8.7kg) | ASTMD1238 | 7.0 | g/10min | |
| 收缩率 | 流动 | ASTMD955 | 0.40到0.60 | % |
| 收缩率 | 横向流动 | ASTMD955 | 0.50到0.70 | % |
| 肖氏硬度 | 邵氏A | ASTMD2240 | 90 | |
| 肖氏硬度 | 邵氏D | ASTMD2240 | 47 | |
| 弯曲模量(3.20mm) | ASTMD790 | 65.9 | MPa | |
| 泰伯耐磨性(1000g,H-22转轮) | ASTMD1044 | 50.0 | mg | |
| 拉伸应力 | 50%应变,3.20mm | ASTMD412 | 6.30 | MPa |
| 拉伸应力 | 100%应变,3.20mm | ASTMD412 | 9.70 | MPa |
| 拉伸应力 | 300%应变,3.20mm | ASTMD412 | 17.9 | MPa |
| 抗张强度(断裂,3.20mm) | ASTMD412 | 38.2 | MPa | |
| 伸长率(断裂,3.20mm) | ASTMD412 | 530 | % | |
| 断裂伸长率(3.20mm) | ASTMD412 | 60 | % | |
| 撕裂强度1(3.20mm) | ASTMD624 | 133 | kN/m | |
| 压缩永久变形 | 25°C,22hr | ASTMD395B | 25 | % |
| 压缩永久变形 | 70°C,22hr | ASTMD395B | 40 | % |
| 玻璃转化温度 | DSC | -34.0 | °C | |
| 维卡软化温度 | ASTMD15252 | 90.6 | °C | |
| 线形热膨胀系数-流动 | ASTMD696 | 1.6E-4 | cm/cm/°C | |
TPU聚醚 2103-90AE TPU塑料供应商,长期销售美国路博润生产的TPU聚醚原料,以上是“TPU聚醚 Estane® 2103-90AE TPU”塑胶料的物性表参数.近期代理商可转仓交易:韩国DAEHA PP TECHLEN M7151 高刚性 汽车领域的应用,汽车外部零件
美国RTP TPU聚脂 RTP 1205-80D 填料,玻璃纤维增强材料,30%填料按重量.
日本CardioTech TPU合金 PolyBlend™ 1100-45A
美国Teknor Apex TPE Telcar® TL-2625C 注射成型,挤出 把手,通用,玩具,消费品应用领域,个人护理,垫圈
美国Star TPE StarFlex® 7092-1003
美国普立万 TPE Dynaflex™ G7980-1 NSFG 良好的着色性,良好的加工稳定性,良好的流动性,可加工性良好,可回收材料,注射成型 密封件,垫圈,家用货品,消费品应用领域,包覆成型,非特定食品应用,柔软的把手,厨具,食品服务领域
美国Teknor Apex TPE Sarlink® TPE ML-1640B BLK (PRELIMINARY DATA)
土耳其Elastron SEBS Elastron® G G100.A50.B 耐化学性良好,嵌段共聚物,可粘结性,柔软,注射成型
比利时Ravago PP+EPDM ENFLEX VL-120-60A
美国RTP PPS RTP 1305.3 P-1 填料,玻璃纤维增强材料,33%填料按重量.
美国普立万 TPE Versaflex™ OM 9-802CL 清晰度高,良好的着色性,注射成型 柔软的把手,包覆成型,柔软触感应用,消费品应用领域
美国Polymer Dynamix PEEK DynaPath™ 3265-E 耐化学性良好,尺寸稳定性良好,挤出 航空航天应用,工业应用,电气/电子应用领域
● TPU聚醚 德国巴斯夫 Elastollan 1185A10V-Film
● TPU聚醚 德国巴斯夫 Elastollan WY1157
水解稳定,耐低温,韧性良好,高耐热性,挤出,注射成型
● TPU聚醚 德国科思创 Desmopan DP 9386A
抗微生物,低温下的柔性,耐水解性,挤出,注射成型
● TPU聚醚 德国科思创 Texin RxT65D
热消毒,韧性良好,辐射消毒,抗撞击性良好,环氧乙烷消毒良好,耐磨损性,水解稳定,良好的柔韧性,挤出,注射成型,吹塑成型
● TPU聚醚 美国路博润 PEARLCOAT 162K