| 注吹成型,注射成型 | |
| 薄膜 | |
| 性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | |
| 比重 | ASTMD792 | 1.14 | g/cm3 | |
| 熔流率(熔体流动速率)(224°C/8.7kg) | ASTMD1238 | 1.2 | g/10min | |
| 收缩率 | 流动 | ASTMD955 | 0.40到0.50 | % |
| 收缩率 | 横向流动 | ASTMD955 | 0.50到0.80 | % |
| 肖氏硬度(邵氏A) | ASTMD2240 | 92 | ||
| 弯曲模量(3.20mm) | ASTMD790 | 65.9 | MPa | |
| 泰伯耐磨性(1000g,H-22转轮) | ASTMD1044 | 50.0 | mg | |
| 拉伸应力 | 50%应变,3.20mm | ASTMD412 | 6.90 | MPa |
| 拉伸应力 | 100%应变,3.20mm | ASTMD412 | 9.70 | MPa |
| 拉伸应力 | 300%应变,3.20mm | ASTMD412 | 20.3 | MPa |
| 抗张强度(断裂,3.20mm) | ASTMD412 | 38.9 | MPa | |
| 伸长率(断裂,3.20mm) | ASTMD412 | 480 | % | |
| 断裂伸长率(3.20mm) | ASTMD412 | 60 | % | |
| 撕裂强度1(3.20mm) | ASTMD624 | 94.6 | kN/m | |
| 压缩永久变形 | 25°C,22hr | ASTMD395B | 25 | % |
| 压缩永久变形 | 70°C,22hr | ASTMD395B | 40 | % |
| 玻璃转化温度 | DSC | -27.0 | °C | |
| 维卡软化温度 | ASTMD15252 | 102 | °C | |
| 线形热膨胀系数-流动 | ASTMD696 | 1.6E-4 | cm/cm/°C | |
TPU聚醚 2103-90AEL TPU塑料供应商,长期销售美国路博润生产的TPU聚醚原料,以上是“TPU聚醚 Estane® 2103-90AEL TPU”塑胶料的物性表参数.近期代理商可转仓交易:中国山东东辰 PP Shandong PP PGF6301 填料,玻璃纤维增强材料,30%填料按重量.电器用具,电气/电子应用领域
沙伯基础 PP LNP™ VERTON™ MV00AS compound
法国阿科玛 PVDF Kynar® 760
美国Techmer TPU HiFill® TPU 0780 高密度,注射成型
德国巴斯夫 TPU聚脂 Elastollan® C 98 A
日本三菱 TPE THERMORUN® 3707N 硬度,低,挤出
美国NOVA TPV NOVALAST® 6001 耐化学性良好,良好的着色性,食品接触的合规性,注射成型,挤出,吹塑成型
美国Teknor Apex TPE Telcar® TL-1377A 挤出,注射成型 吹塑成型应用,汽车领域的应用,汽车外部零件,耐候性密封条,垫圈,汽车外部装饰,汽车内部零件,通用
德国凯柏胶宝 TPE THERMOLAST® M TM9HET (Series: MC/HE)
英国ELASTO SEBS Dryflex® A1 602501
中国苏州特威塑胶 PP+EPDM New-prene™ 6165B
意大利Versalis EVA Greenflex® FD 53
美国RTP PEI RTP 2187 L 填料,碳纤维增强材料,40%填料按重量.
大日本油墨 PPS DIC.PPS FZ-3500 填料,玻璃纤维增强材料.
● TPU聚醚 德国巴斯夫 Elastollan 1185A10V-Film
● TPU聚醚 德国巴斯夫 Elastollan WY1157
水解稳定,耐低温,韧性良好,高耐热性,挤出,注射成型
● TPU聚醚 德国科思创 Desmopan DP 9386A
抗微生物,低温下的柔性,耐水解性,挤出,注射成型
● TPU聚醚 德国科思创 Texin RxT65D
热消毒,韧性良好,辐射消毒,抗撞击性良好,环氧乙烷消毒良好,耐磨损性,水解稳定,良好的柔韧性,挤出,注射成型,吹塑成型
● TPU聚醚 美国路博润 PEARLCOAT 162K