性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | |
比重 | ASTMD792 | 1.33 | g/cm3 | |
熔流率(熔体流动速率)(300°C/1.2kg) | ASTMD1238 | 15 | g/10min | |
收缩率-流动 | ASTMD955 | 0.20to0.40 | % | |
拉伸模量(3.20mm,注塑) | ASTMD638 | 4000 | MPa | |
TensileStrength(Break,3.20mm,InjectionMolded) | ASTMD638 | 100 | MPa | |
TensileElongation(Break,3.20mm,InjectionMolded) | ASTMD638 | 4.0 | % | |
悬壁梁缺口冲击强度(23°C,3.20mm,注塑) | ASTMD256 | 110 | J/m | |
载荷下热变形温度(0.45MPa,未退火) | ASTMD648 | 145 | °C | |
载荷下热变形温度(1.8MPa,未退火) | ASTMD648 | 140 | °C | |
载荷下热变形温度(1.8MPa,退火) | ASTMD648 | 143 | °C | |
表面电阻率 | ASTMD257 | 3.0E+14 | ohms | |
VolumeResistivity(1.80mm) | ASTMD257 | 1.0E+16 | ohmscm | |
介电强度(1.60mm) | ASTMD149 | 27 | kV/mm | |
DielectricConstant(1.60mm,1MHz) | ASTMD150 | 3.10 | ||
漏电起痕指数(3.00mm) | IEC60112 | 175 | V | |
FlameRating2(1.5mm) | UL94 | V-0 |
PC PC 8702-15 (NA)塑料供应商,长期销售美国盛禧奥生产的PC原料,以上是“PC EMERGE™ PC 8702-15 (NA)”塑胶料的物性表参数.近期代理商可转仓交易:意大利Versalis EVA Greenflex® FD 23
意大利SO.F.TER SBS Sofprene T® 550100A55 注射成型
日本东丽 PPS Torelina® A504X90 填料,玻璃纤维增强材料,40%填料按重量.
沙伯基础 PEI ULTEM™ D9065 resin
中国余姚腾龙塑化 PPO(PPE) Yuyao PPO N120A 阻燃性,无卤,韧性良好,收缩性低,良好的电气性能,尺寸稳定性良好,高刚性,良好的流动性,注射成型 电气元件,连接器
美国RTP LCP RTP 3400 G-540 填料,玻璃纤维增强材料.
比利时Ravago PC+ABS Mablex 459 通用,高光 通用
巴西Unigel PC Duroloy® AS-41 耐低温冲击,流动性中等,注射成型 电气/电子应用领域,汽车领域的应用
美国Entec PC Hylex® P1010FRMA 阻燃性,通用 通用
日本三菱 PC Iupilon® EGN2020R2 填料,玻璃纤维增强材料,20%填料按重量.
日本三菱 PBT NOVADURAN® 5010TRXA 冲击改性,注射成型
以色列屹立 PA66 6/POLYNIL® C50 复合 复合
美国RheTech PA66 Rhelon X2000-00 注射成型
以色列普利朗 PA66 PLUSTEK RA353M8 填料,矿物填料,40%填料按重量.
美国The Plastics PA66 Polifil® Nylon 627LP
● PC 美国RTP 384 HEC TFE 15
注塑
● PC 沙伯基础 LNP THERMOCOMP Lexan_JK500 compound
填料:玻璃纤维增强材料, 10% 填料按重量。
● PC 日本三菱 Iupilon GSH2020DF
填料:玻璃纤维增强材料, 20% 填料按重量。
● PC LG化学 1261-03
抗撞击性,良好耐热性,高清晰度,高食品接触的合规性
● PC 沙伯基础 LEXAN XHT3143T resin