性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | |
比重 | ASTMD792 | 0.900 | g/cm3 | |
熔流率(熔体流动速率)(230°C/2.16kg) | ASTMD1238 | 3.2 | g/10min | |
薄膜厚度-经测试 | 50 | um | ||
膜刺穿强度(50um) | ASTMD5748 | 0.500 | J | |
膜刺穿力(50um) | ASTMD5748 | 42.0 | N | |
割线模量 | 2%正割,MD:50um | ASTMD882 | 1170 | MPa |
割线模量 | 2%正割,TD:50um | ASTMD882 | 1140 | MPa |
抗张强度 | MD:屈服,50um | ASTMD882 | 27.0 | MPa |
抗张强度 | TD:屈服,50um | ASTMD882 | 41.0 | MPa |
抗张强度 | MD:断裂,50um | ASTMD882 | 38.0 | MPa |
抗张强度 | TD:断裂,50um | ASTMD882 | 39.0 | MPa |
伸长率 | MD:断裂,50um | ASTMD882 | 250 | % |
伸长率 | TD:断裂,50um | ASTMD882 | 6.0 | % |
落锤冲击(50um) | ASTMD1709A | 50 | g | |
埃尔曼多夫抗撕强度 | MD:50um | ASTMD1922 | 14 | g |
埃尔曼多夫抗撕强度 | TD:50um | ASTMD1922 | 24 | g |
薄膜厚度-经测试 | 50 | um | ||
膜刺穿强度(50um) | ASTMD5748 | 0.500 | J | |
膜刺穿力(50um) | ASTMD5748 | 42.0 | N | |
割线模量 | 2%正割,MD:50um | ASTMD882 | 1170 | MPa |
割线模量 | 2%正割,TD:50um | ASTMD882 | 1140 | MPa |
抗张强度 | MD:屈服,50um | ASTMD882 | 27.0 | MPa |
抗张强度 | TD:屈服,50um | ASTMD882 | 41.0 | MPa |
抗张强度 | MD:断裂,50um | ASTMD882 | 38.0 | MPa |
抗张强度 | TD:断裂,50um | ASTMD882 | 39.0 | MPa |
伸长率 | MD:断裂,50um | ASTMD882 | 250 | % |
伸长率 | TD:断裂,50um | ASTMD882 | 6.0 | % |
落锤冲击(50um) | ASTMD1709A | 50 | g | |
埃尔曼多夫抗撕强度 | MD:50um | ASTMD1922 | 14 | g |
埃尔曼多夫抗撕强度 | TD:50um | ASTMD1922 | 24 | g |
溶融温度(DSC) | 内部方法 | 162到166 | °C | |
光泽度(45°,50.0um) | ASTMD2457 | 32 | ||
雾度(50.0um) | ASTMD1003 | 23 | % |
PP 227塑料供应商,长期销售美国盛禧奥生产的PP原料,以上是“PP INSPIRE™ 227”塑胶料的物性表参数.近期代理商可转仓交易:韩国GS加德士 PP Caltex PP HC43 阻燃性,高耐热性,高光,高刚性 电气/电子应用领域
中国山东华夏神舟新材 氟橡胶 Huaxia Shenzhou FKM DS2601-2
美国RTP TPU聚脂 RTP 1200.5-90A
伊朗Asia Technology TPO ATPioneers PP CAP101
● PP 利安德巴塞尔 BA753AC
中等熔体流动良好的综合性能和加工热稳定性好,
● PP 沙特sabic 108MF10
抗冲击,抗紫外线
● PP 沙伯基础(原GE) MFB71L
玻璃珠增强,玻纤增强,注塑
● PP 利安德巴塞尔 EKC 133N KF
矿物填料, 16% 填料按重量、改良抗撞击性、低光泽、流动性高、耐刮擦性
● PP 利安德巴塞尔 PD702NW
刚性良好,均聚物, 抗静电性,流动性高。应用于薄壁容器,食品容器。注射成型