性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | |
密度 | ASTMD1505 | 0.925 | g/cm3 | |
熔流率(熔体流动速率)(190°C/2.16kg) | ASTMD1238 | 2.2 | g/10min | |
摩擦系数(铸造薄膜) | ASTMD1894 | 0.15 | ||
薄膜厚度-经测试 | 32 | um | ||
氧气传输速率(32um,铸造薄膜) | ASTMD3985 | 6300 | cm3/m2/24hr | |
水气透过率(32um,铸造薄膜) | ASTMF1249 | 14 | g/m2/24hr | |
DartDropTest2(31.8um) | ASTMD1709 | 30.9 | kN/m | |
ElmendorfTearStrength2 | MD:31.8um | ASTMD1922 | 73.4 | kN/m |
ElmendorfTearStrength2 | TD:31.8um | ASTMD1922 | 98.5 | kN/m |
薄膜厚度-经测试 | 32 | um | ||
氧气传输速率(32um,铸造薄膜) | ASTMD3985 | 6300 | cm3/m2/24hr | |
水气透过率(32um,铸造薄膜) | ASTMF1249 | 14 | g/m2/24hr | |
DartDropTest2(31.8um) | ASTMD1709 | 30.9 | kN/m | |
ElmendorfTearStrength2 | MD:31.8um | ASTMD1922 | 73.4 | kN/m |
ElmendorfTearStrength2 | TD:31.8um | ASTMD1922 | 98.5 | kN/m |
维卡软化温度 | ASTMD1525 | 98.3 | °C | |
熔融峰值温度 | ASTMD3418 | 111 | °C | |
光泽度(60°,31.8um,铸造薄膜) | ASTMD2457 | 135 | ||
雾度(31.8um,铸造薄膜) | ASTMD1003 | 4.0 | % |
LDPE 5440塑料供应商,长期销售美国雪佛龙菲利普斯生产的LDPE原料,以上是“LDPE MarFlex® 5440”塑胶料的物性表参数.近期代理商可转仓交易:德国爱彼斯 PP均聚 ALTECH® PP-H FC 4940/100 MR40 填料,ALBIS,德国爱彼斯.厨具
美国KMI PP均聚 KMI PP KM-008IB
台湾台化 PP均聚 YUNGSOX® PP 1009 可更新资源,高耐热性,注射成型,树脂传递成型 电气元件,工程配件
瑞典柏力开米 PP均聚 POLYfill PPH T5060 填料,矿物填料,60%填料按重量.
匈牙利Inno-Comp PP共聚 INNOPOL® PP CS 2-3840 MO 填料,玻璃纤维增强材料,40%填料按重量.
瑞典柏力开米 PP均聚 POLYfill PPH GF4030 PD2 填料,玻璃纤维增强材料,30%填料按重量.
意大利Taro Plast PP共聚 HAIPLEN EP10 G2 BA 填料,玻璃纤维增强材料,10%填料按重量.
加拿大ACLO PP共聚 ACCUTECH™ CP0436G10M20CL 填料,ACLO,加拿大ACLO.
巴西布拉斯科 LLDPE Braskem PE SLH118
美国利安德巴塞尔 HDPE Alathon® M5372
奥地利北欧化工 HDPE Borcoat™ HE3450
上海华合 PBT PBT-30GF 30%玻纤增强
瑞典ELASTO TPE WS 30M500 可回收材料耐化学性良好耐气候影响性能良好 建筑材料,建筑应用领域,密封剂,汽车领域的应用,水箱,装配玻璃
蒲城能源 LLDPE DFDA-7042 其它
● LDPE 伊朗石化 2420H 其它
● LDPE 英力士 PH23T630
良好的灵活性
● LDPE 美国利安德巴塞尔 Petrothene NA952000
● LDPE 台湾化纤 6334F
低密度、高光滑性、 可加工性,良好、一般目的、中等抗结块性
● LDPE 利安德巴塞尔 E GGNX 23-D022
良好的耐化学性,良好的耐蚀性,良好的加工,高级文化权利(应力裂纹抗拒),高强度