| 性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | |
| 比重 | ASTMD792 | 1.20 | g/cm3 | |
| 熔流率(熔体流动速率)(300°C/1.2kg) | ASTMD1238 | 18 | g/10min | |
| 收缩率-流动(3.20mm) | InternalMethod | 0.50to0.70 | % | |
| 吸水率(24hr) | ASTMD570 | 0.15 | % | |
| 室外适用性 | UL746C | f1 | ||
| 抗张强度2(屈服) | ASTMD638 | 62.1 | MPa | |
| 伸长率2(断裂) | ASTMD638 | 130 | % | |
| 弯曲模量4(50.0mm跨距) | ASTMD790 | 2340 | MPa | |
| 弯曲强度4(屈服,50.0mm跨距) | ASTMD790 | 96.5 | MPa | |
| 悬壁梁缺口冲击强度(23°C) | ASTMD256 | 690 | J/m | |
| 装有测量仪表的落镖冲击(23°C,EnergyatPeakLoad) | ASTMD3763 | 62.1 | J | |
| 落锤冲击(23°C) | InternalMethod | 169 | J | |
| 拉伸冲击强度4 | ASTMD1822 | 473 | kJ/m2 | |
| 载荷下热变形温度(1.8MPa,未退火,6.40mm) | ASTMD648 | 129 | °C | |
| RTIElec | UL746 | 130 | °C | |
| RTIImp | UL746 | 125 | °C | |
| RTIStr | UL746 | 125 | °C | |
| 相比耐漏电起痕指数(CTI) | UL746 | PLC2 | ||
| 高电弧燃烧指数(HAI) | UL746 | PLC1 | ||
| 高电压电弧起痕速率(HVTR) | UL746 | PLC2 | ||
| 热丝引燃(HWI) | UL746 | PLC4 | ||
| UL阻燃等级(1.5mm) | UL94 | HB | ||
| 透射率(2540um) | ASTMD1003 | 88.0 | % | |
PC LS1 resin塑料供应商,长期销售沙伯基础生产的PC原料,以上是“PC LEXAN™ LS1 resin”塑胶料的物性表参数.近期代理商可转仓交易:德国TechnoCompound TPE TechnoElast V A9000 I 2 sw
荷兰Wittenburg SEBS Cawiton® SN970 嵌段共聚物,注射成型
意大利SO.F.TER SBS Sofprene T® 540200A30 注射成型
美国Techmer PEEK HiFill® PEEK CF30 A 002 填料,碳纤维增强材料.
日本宝理 PPS DURAFIDE® 1130A1 填料,玻璃纤维增强材料,30%填料按重量.
意大利Guarniflon PTFE Flontech® FT-GL15-1 填料,玻璃纤维增强材料,15%填料按重量.
美国RTP PPA RTP 4011 A 填料,玻璃纤维增强材料,60%填料按重量.
沙伯基础 PPO(PPE) NORYL™ WCD801AU resin
德国爱彼斯 POM共聚 ALCOM® POM 770/1 Si2 热稳定性,耐磨损性良好,共聚物 汽车领域的应用,车轮,机器/机械部件,齿轮,轴承
德国TEKUMA POM共聚 Tekuform C9
美国PlastxWorld PC Verolloy S3500 阻燃性,高耐热性,注射成型
美国盛禧奥 PC PULSE™ 2300 PT
韩国乐喜 PC Lucky Enpla LAY1000 通用,注射成型 电气/电子应用领域,汽车领域的应用,外壳
意大利Taro Plast PC TAROBLEND 46 流动性高,注射成型
美国杜邦 PBT Crastin® S650FR BK851 阻燃性,注射成型
● PC 美国RTP RTP ESD 383
填料:碳纤维增强材料, 20% 填料按重量。
● PC 日本帝人 Panlite LN-1010RM
阻燃性,反射率高,注射成型
● PC 美国盛禧奥 CALIBRE 301-6
● PC 美国RTP RTP 300 TFE 10 SE A
无溴,自熄,Chlorine/free,润滑,注射成型
● PC 沙伯基础(原GE) 3412ECR resin
玻璃纤维增强材料, 20% 填料按重量。Chlorine Free; 刚性,高;无溴;阻燃性