性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | |
密度 | ASTMD4883 | 0.949 | g/cm3 | |
熔流率(熔体流动速率) | 190°C/21.6kg | ASTMD1238 | 8.5 | g/10min |
熔流率(熔体流动速率) | 190°C/5.0kg | ASTMD1238 | 0.30 | g/10min |
抗环境应力开裂(100%Igepal,F50) | ASTMD1693C | >5000 | hr | |
抗张强度2(屈服) | ASTMD638 | 24.1 | MPa | |
抗张强度2(断裂) | ASTMD638 | 30.3 | MPa | |
伸长率2(屈服) | ASTMD638 | 10 | % | |
伸长率2(断裂) | ASTMD638 | >600 | % | |
弯曲模量-2%正割 | ASTMD790A | 896 | MPa | |
流体静力学设计基础 | 23°C | ASTMD2837 | 11.0 | MPa |
流体静力学设计基础 | 60°C | ASTMD2837 | 6.89 | MPa |
悬壁梁缺口冲击强度 | ASTMD256 | 640 | J/m | |
NotchedIzodImpact(Area) | ASTMD256 | 63.0 | kJ/m2 | |
肖氏硬度(邵氏D) | ASTMD2240 | 64 | ||
脆化温度 | ASTMD746 | <-118 | °C | |
维卡软化温度 | ASTMD1525 | 126 | °C | |
氧感应时间(210°C) | ASTMD3895 | >20 | min | |
热稳定性 | ASTMD3350 | >240 | °C | |
补充信息 | TestMethod | NominalValue | Unit | |
CellClassification | ASTMD3350 | 445574C | ||
MinimumRequiredStrength | ISO9080 | 10.0 | MPa | |
PENT-NotchTensile | ASTMF1473 | >10000 | hr |
HDPE INEOS HDPE TUB 121N塑料供应商,长期销售瑞士英力士生产的HDPE原料,以上是“HDPE INEOS HDPE TUB 121N”塑胶料的物性表参数.近期代理商可转仓交易:美国利安德巴塞尔 PP均聚 Moplen HP528N
加拿大ACLO PP均聚 ACCUTECH™ HP0334T20L 填料,ACLO,加拿大ACLO.
瑞士英力士 PP均聚 INEOS PP 401-CA55
巴西布拉斯科 PP均聚 Braskem PP C104-01 食品接触的合规性,抗冲共聚物,刚性良好,耐低温冲击,热成型,挤出
奥地利北欧化工 PP均聚 Beta (o)-PP™ BE60-7032
韩国SK化学 PP共聚 YUPLENE® R520Y
美国利安德巴塞尔 PP共聚 Hostacom CR 1171 G1 G74010
法国SILON PP共聚 TABOREN® PC 62 G 20-071 填料,玻璃纤维增强材料.
美国M.Holland LLDPE MTEGRITY™ LLDPE LL204AA 低密度,良好的强度,韧性良好,流延薄膜 混合,流延薄膜
美国RheTech PP共聚 RheTech Polypropylene F43-01A 填料,玻璃矿物,35%填料按重量.
美国华美化学 LLDPE Westlake LLDPE LF2010
日本三井 HDPE LUBMER™ L5220 润滑,高摩擦 汽车内部零件,轴承,齿轮
澳大利亚凯诺斯 HDPE Qenos PE HD1099UV
韩国大韩油化 HDPE HIDEN® P600 良好的抗蠕变性 管道系统
上海华合 PBT PBT+MD40 40%无机物增强.
● HDPE 日本三井 LUBMER L5000
抗撞击性良好,降噪良好,耐磨损性,低摩擦系数
● HDPE 美国RTP RTP 799 X 112538
抗静电性,吹塑成型
● HDPE 美国英力士 B53-35H-100
高荷载强度和良好的环境应力抗裂性。
● HDPE 英力士 B4020LG/34
低气味,良好的耐热性,良好的耐冲击性,良好抵抗应力开裂
● HDPE 乐天化学 2600F
高的加工性能